Problem: Abrasive wear of Franklin Mint's dies caused deterioration that slowed release rates. Die hangups and machine jams became a serious source of production downtime. Burring and defacing of dies also boosted reject rates. Conventional coatings were tried on both the male and female dies without success. Solution: MAGNAGOLD coating provides dies with a permanently dry lubricated and wear resistant surface, eliminating hangups, machine jams, and burring problems. Reject rates dropped to practically zero.
|